RUS   ENG
Home Contacts

Ê-200 H FC

PRODUCT TYPE
weak-acid cation exchange resin.

 
APPLICATION:

K-200 H FC differs in dispersion of particle size, has high total exchange capacity, chemical stability, osmotic stability and considerable economic profit during steam production.

This type is especially suitable for desalinization of industrial water, binding of alkaline ions, extraction of heavy metals (Cu, Ni, Zn) in hydrometallurgy.


PHYSICAL AND CHEMICAL PARAMETERS

Appearance opaque beige beads
Structure macroporous
Polymer matrix polystyrene - divinylbenzene
Functional group carboxylic acid
Ion form H+
Moisture, % 47
Dynamic exchange capacity, mole/m3 2037
Total exchange capacity, meq/ml3 4,3
Bulk density, g/ml 0,79
Specific density, g/ml 1,20
Specific volume, cm3/g 2,77
Particle size*, mm 0,50-0,70
Effective particle size, mm 0,52
Uniformity coefficient 1,48
Volumetric part of fraction, % 99
Filtrate oxidation, mg/g 0,15
Content of Cl ions, g/cm3 -
Content of Fe, g/cm3 -
Storage period, year 2
Storage temperature, îÑ -20… +120

*Fraction size is shown at the diagram



RECOMMENDED RATES AT OPERATION PROCESS

Max. process temperature, îÑ 75
Process range of acidity, ðÍ 5-14
Layer height, mm 800
Linear speed at operation, m/h 10-15


RECOMMENDED RATES AT REGENERATION PROCESS

Regenerating media (RM) HCl H2SO4
Quantity of RM, g RM/l of resin 70 90
RM Concentration, % 3-6 0,5-0,8
Consumption of regeneration, RM volume/ resin volume 2-3:1 15-20:1
Linear speed at regeneration process, m/h 5-20
Contact period at regeneration process, min. 30
Linear speed at washing process, m/h 5-20
Contact period of washing process, min. 20-40
Volume changing, Í+→Ñà2+, % +7


INTERNATIONAL EQUIVALENTS

Purolite C-105, Lewatit CNP-80, Amberlite IRC-84/86, Russian standard ÊÁ-4
PACKING

Polypropylene bag with polyethylene liner. Net weight is 25 kg.